Coating type: high cellulose
Tensile strength, MPA: 450-550- (65-80)
Yield point, MPa: 400-450 (58-65)
Relative elongation, %: 22-24
Not recommended to bake before welding
Welding current strength, A for electrodes with a diameter of, mm (in)
2.5 (3/32) - 50-90
3.2 (1/8) - 80-120
4.0 (5/32) - 120-160
Welding should be performed with DC of reversed polarity “+” on an electrode with an arc voltage of 23-27 V.